Corrigendum: Highly Active N,O Zinc Guanidine Catalysts for the Ring-Opening Polymerization of Lactide
An error in the units of kp in Table 1 was found. The units should be 10−2 s−1 m−1 instead of 10−12 s−1 m−1.
Init. |
kp[b] [10−2 s−1 m−1] |
kapp[c] [10−4 s−1] |
Conv.[d] [%] |
Mtheo[e] [g mol−1] |
Mn[e] [g mol−1] |
Mw[e] [g mol−1] |
---|---|---|---|---|---|---|
C1 |
9.5±1.6 |
1.26±0.07 |
52±2 |
37 400 |
49 400 |
69 100 |
C2 |
8.2±1.2 |
1.09±0.10 |
52±2 |
37 400 |
35 000 |
49 000 |
C3 |
6.3±0.6 |
1.01±0.10 |
53±2 |
38 200 |
46 900 |
70 400 |
C4 |
7.1±1.1 |
1.03±0.15 |
55±2[45] |
39 600 |
42 600 |
68 100 |
- [a] Conditions: 90 min, [M]/[I]=500, 150 °C, solvent free, technical LA (no further purification). [b] Determined by plotting kapp versus [I]. kp [I] [M]=kapp [M]; kp=kapp/[I] [c] Determined from the slope of the plots of ln([LA]0/[LA]t) versus time. [d] As determined by 1H NMR spectroscopy. [e] Determined by GPC (in THF), Mn, theo: 72 000 g mol−1 for 100 % conversion. [f] Polymerization with tin(II) 2-ethylhexanoate: 90 min., conv.=94 %, Mn=114 700 g mol−1, PD=2.0.
The authors and the editorial office apologize for this oversight and for any inconvenience caused.